Step-by-step procedure Glass-ceramic restoration case
1.Preoperative situation : Fractured tooth.
2.Preparation of tooth 11 for an IPS e.max CAD crown and of tooth 21 for an IPSe.max Ceram veneer.
3.After milling the e.max CAD MO block, the crystallization process is conducted in a ceamic furnace.
The framework obtains its natural shade through the crystallization process.
The tooth-coloured framework is subsequently veneered with IPS e.max Ceram layering ceramic.
Step-by-step procedure Zirconium oxide restoration case
1.Preoperative situation
2.IPS e.max ZirCAD crown preparation, performed with the help of a silicone matrix.
3.The IPS e.max ZiCAD blocks are processed in the inLab sysrem in a partially sintered. The milled framework is subsequently sintered in the Sintramat high temperature furnace.
Either IPS e.max ZirPress is pressed onto the crown coping and/or the crown coping is veneered using IPS e.max Ceram layering ceramic.
4.Conditioning of the preparation:
Clean preparation with prophy paste, rinse with water and blow dry with the air syringe.